GC INITIAL® IQ ONE SQIN – System Set, 228 g – #877098
Description
Paintable Color-and-form ceramic system for aesthetic finishing of monolithic or minimally buccally reduced frameworks made of zirconia or lithium disilicate, designed to achieve high aesthetics with significant time savings. (GC)
What’s included (quantities & sizes)
10× SPS Stain (SPS-1 / 2 / 7 / 8 / 13 / 14 / 17 / 18 / 19 / 20), 3 g
1× SPS Glaze Fluo (GL-FLUO), 10 g
1× SPS Glaze Liquid, 25 mL
2× IQ LP ONE LUSTRE PASTE Neutral (L-N / L-NFL), 4 g
4× IQ LP ONE LUSTRE Body Shade (L-A / B / C / D), 4 g
6× IQ LP ONE Enamel Effect Shade (L-3 / 6 / 8 / 9 / 10 / OP), 4 g
1× IQ LP ONE/NF Diluting Liquid, 8 mL
1× IQ LP ONE/NF Refresh Liquid, 8 mL
5× IQ SQIN Powder Dentin (Body A / B / C / D / BL-D), 10 g
5× IQ SQIN Powder Enamel (E-57 / 58 / 59 / 60 / BL-E), 10 g
1× IQ SQIN Powder Translucent Opal Booster (TO), 10 g
3× IQ SQIN Powder GUM (light / dark / neutral), 10 g
1× IQ SQIN Form & Texture Liquid, 25 mL
Accessories: 1× IQ LP ONE Mixing Dish, 1× IQ LP ONE Brush 00, 1× IQ LP ONE Brush 2, 1× IQ LP ONE Plastic Cover
Documentation: 1× IQ ONE SQIN Technical Manual, 1× IQ LP ONE Colour Chart, 1× SPS Colour Chart
Firing schedules (guideline values)
Monolithic frameworks (LUSTRE Pastes ONE firing)
| Material | Start temp | Drying | Vacuum | Heat rate | Firing temp | Hold |
|---|---|---|---|---|---|---|
| Lithium disilicate | 450°C | 4 min | Yes | 45°C/min | 735–760°C | 1 min |
| Zirconia | 450°C | 6 min | Yes | 45°C/min | 800–900°C | 1 min |
Buccally reduced frameworks – Step 1 (Individualization & connection firing with LUSTRE Pastes ONE)
| Material | Start temp | Drying | Vacuum | Heat rate | Firing temp | Hold |
|---|---|---|---|---|---|---|
| Lithium disilicate | 450°C | 4 min | Yes | 45°C/min | 760°C | 1 min |
| Zirconia | 450°C | 6 min | Yes | 45°C/min | 850°C | 1 min |
Buccally reduced frameworks – Step 2 (Form & texture using IQ SQIN)
| Material | Start temp | Drying | Closing | Vacuum | Heat rate | Firing temp | Hold |
|---|---|---|---|---|---|---|---|
| Lithium disilicate | 400°C | 4 min | 4 min | Yes | 40°C/min | 740–780°C | 1 min |